4140 alyaj chalè trete wonn ba


4140 cho woule chalè trete wonn ba
4140 se yon asye lajman itilize kabòn asye . Li se yon alyaj objektif jeneral ak bon fòs, severite ak dite . yo rele li chrome-molibdèn asye paske li gen 0 . 95% CHROMIUM ak 0.20% eleman alyaj.
4140 Chalè ki ka trete alyaj se yon CHROMIUM-MOLYBDENUM MEDIM CARBON ALLOYE 26-32 epi li se estrès soulajman pou misyon pou minimize warping pandan pwosesis . Dite lokal kapab tou jwenn nan flanm dife oswa endiksyon redi . 4140 se sitou itilize nan koube machin mouri ak se tou yon chwa ideyal pou aplikasyon ki mande pou pi wo severite pase asye modere {{{ Plak ejector, kranpon, enstalasyon, plak kout pyen, kolye fè egzèsis, akoupleman, aks, tiyo, rasin machin, kò reamer, blòk machin .
Gnee 4140 alyaj cho woule wonn bar spesifikasyon
AISI 4140 Hot-woule Round Bar: Comprehensive Table Property
|
Kategori pwopriyete |
Paramèt |
Espesifikasyon teknik |
|---|---|---|
|
Dimansyon debaz yo |
Range dyamèt (mm) |
20 - 300 |
|
Ranje longè (m) |
3 - 12 (tolerans koupe-a-longè:+50⁄-0mm) |
|
|
Nòm tolerans |
Tolerans dyamèt |
± 0.8% (ASTM) / ± 0.6% (DIN) / ± 1.0% (GB) |
|
Ovalite |
Mwens pase oswa egal a 0.8% nan dyamèt |
|
|
Pwopriyete sifas yo |
Metòd Tretman |
Mill echèl sifas / vire / sandblasted |
|
Brutality (ra) |
12.5 - 25 μm (echèl moulen) / 3.2 - 6.3 μm (vire) |
|
|
Pwopriyete fizik |
Dite (HB) |
197 - 241 (cho-woule) / 280 - 350 (Q&T) |
|
Densite |
7.85 g/cm³ |
|
|
Konpozisyon materyèl |
Konpozisyon chimik (%) |
C: 0.38-0.43, Cr: 0.80-1.10, Mo: 0.15-0.25, Mn: 0.75-1.00, Si: 0.15-0.35 |
|
Pite |
Enklizyon mwens pase oswa egal a klas 2 (ASTM E45), S/P mwens pase oswa egal a 0.035% |
|
|
Nòm Nwayo |
Nòm entènasyonal yo |
ASTM A322 Gr .4140 / en 10083-1 42 CRMO4 / GB / T 3077 42 CRMO |
4140 alyaj cho woule chalè trete ba konpozisyon chimik:
| Kabòn: | 0.38/0.43 |
| CHROMIUM: | 0.80/1.00 |
| Molybdenum: | 0.15/0.25 |
| Manganèz: | 0.75/1.00 |
| Silisyòm: | 0.15/0.35 |
| Fosfò: | 0.035 max |
| Souf: | 0.040 Max |
Gnee 4140 alyaj cho woule chalè trete orè ba
4140 alyaj cho woule chalè trete ba (pous)
| 1/2 | 1-7/8 | 3-1/2 | 6-1/4 | 9 | 14 |
| 5/8 | 2 | 3-3/4 | 6-1/2 | 9-1/2 | 16 |
| 3/4 | 2-1/8 | 4 | 6-3/4 | 9-3/4 | |
| 7/8 | 2-1/4 | 4-1/4 | 7 | 10 | |
| 1 | 2-3/8 | 4-1/2 | 7-1/4 | 10-1/2 | |
| 1-1/8 | 2-1/2 | 4-3/4 | 7-1/2 | 11 | |
| 1-1/4 | 2-5/8 | 5 | 7-3/4 | 11-1/4 | |
| 1-3/8 | 2-3/4 | 5-1/4 | 8 | 11-1/2 | |
| 1-1/2 | 2-7/8 | 5-1/2 | 8-1/4 | 12 | |
| 1-5/8 | 3 | 5-3/4 | 8-1/2 | 13 | |
| 1-3/4 | 3-1/4 | 6 | 8-3/4 | 13-1/2 |
Anviwònman GNEE Faktori Gwoup
Gnee Group 4140 cho woule chalè trete anviwònman faktori

Gnee Group 4140 Chalè trete wonn anbalaj ba
Gnee Group 4140 cho woule wonn anbalaj ba

Gnee Gwoup Tès
Gnee Group 4140 alyaj cho woule ht wonn bar tès

FAQ
Èske 4140 alyaj asye korozyon rezistan?
Malgre ke 4140 asye gen CHROMIUM amelyore rezistans korozyon, li pa trè rezistan a korozyon . penti ki apwopriye oswa mezi pwoteksyon yo rekòmande pou itilize nan anviwònman korozivite .
Ki diferans ki genyen ant 4140 ak 4340 asye alyaj?
4140 Steel gen yon kontni kabòn pi ba pase 4340 asye, fè li pi fasil nan machin . Sepandan, 4340 asye gen pi wo fòs ak severite, espesyalman nan pi gwo seksyon, epi li se souvan yo itilize nan aplikasyon lou-devwa .
Èske 4140 asye alyaj dwe soude?
Wi, 4140 asye ka soude lè l sèvi avèk teknik yo soude apwopriye ak prekosyon . Sepandan, pòs-Weld tretman chalè ka oblije retabli pwopriyete li yo, espesyalman nan zòn nan chalè ki afekte .